Mike has a reputation beyond reputeMike has a reputation beyond reputeMike has a reputation beyond reputeMike has a reputation beyond reputeMike has a reputation beyond reputeMike has a reputation beyond reputeMike has a reputation beyond reputeMike has a reputation beyond reputeMike has a reputation beyond reputeMike has a reputation beyond reputeMike has a reputation beyond repute
Default

correct. minimum temp I can cure at is 380, or 193 C. It depends on the plastic formulation.

Corvette wheel center caps, which are marked PPA+PA (I think), don't melt at 380. Nissan centercaps which are ABS melt at about 200F, Honda ones melt at 180. Corvette engine covers can handle the heat, Nissan melt at 220. LS plastic manifolds, as well as FAST composite manifolds can be powdercoated and handle the heat. Its all trial and error
__________________
NISSAN: 75 280Z / 86 300ZX GLL /87 Sentra SE / 03 350Z / 23 Z
Porsche: 93 968 / 23 Macan GTS / 93 968
Mike is offline   Reply With Quote